PC日本出光IR2200物性測(cè)試數(shù)據(jù):
原料技術(shù)數(shù)據(jù)
性能項(xiàng)目 |
試驗(yàn)條件[狀態(tài)] |
測(cè)試方法 |
測(cè)試數(shù)據(jù) |
數(shù)據(jù)單位 |
基本性能 |
熔體流動(dòng)速率 |
300℃ 1.2kg |
ISO 1133 (ASTM D-1238) |
12 |
g/10min |
密度 |
|
ASTM D-792 |
1.2 |
g/cm3 |
吸水率 |
23℃水中24h |
ASTM D-570 |
0.23 |
% |
物理性能 |
光線透過率 |
3mm厚 |
ASTM D-1003 |
85-89 |
% |
機(jī)械性能 |
IZOD沖擊強(qiáng)度 |
4mm with notch 3.2mm with notch |
ISO 180 (ASTM D-256) |
70 |
KJ/m2 |
撓曲彈性率 |
|
ISO 178 (ASTM D-790) |
2350 |
MPa |
泰伯磨耗量 |
1,000round |
ASTM D-1044 |
12 |
mg |
引張降伏強(qiáng)度 |
|
ISO R-527 (ASTM D-638) |
64 |
MPa |
撓曲強(qiáng)度 |
|
ISO 178 (ASTM D-790) |
93 |
MPa |
引張彈性率 |
|
ISO R-527 (ASTM D-638) |
2300 |
MPa |
洛氏硬度 |
|
ISO 2039-2 (ASTM D-785) |
120 |
R |
引張破壞強(qiáng)度 |
|
ISO R-527 (ASTM D-638) |
68 |
MPa |
引張破壞伸率 |
|
ISO R-527 (ASTM D-638) |
115 |
% |
加工性能 |
成形收縮率 |
|
ASTM D-955 |
0.5-0.7 |
% |
熱性能 |
維卡軟化點(diǎn) |
|
ISO 306 |
148 |
℃ |
燃燒性 |
1.47mm厚 |
UL-94 |
V-2 |
|
線膨脹系數(shù) |
|
ASTM D-696 (ASTM D-695) |
6.5 |
×10-5cm/cm/℃ |
熱變形溫度 |
1.8Mpa 18.6kg/cm2 |
ISO 75 (ASTM D-648) |
132 |
℃ |