LCP日本住友化學(xué) E5006L LCP塑膠原料
性能項(xiàng)目 | 測試條件 | 測試方法 | 數(shù)值/描述 | 單位 | |
機(jī)械性能 | 拉伸強(qiáng)度(引張強(qiáng)度) | ASTM D638/ISO 527 | kg/cm2(MPa)[Lb/in2] | ||
拉伸模量 | ASTM D638/ISO 527 | kg/cm2(MPa)[Lb/in2] | |||
拉伸屈服伸長率(延伸率) | ASTM D638/ISO 527 | % | |||
拉伸斷裂伸長率(延伸率) | ASTM D638/ISO 527 | 4.5 | % | ||
彎曲模量(彎曲彈性率) | ASTM D790/ISO 178 | 14200 | kg/cm2(MPa)[Lb/in2] | ||
彎曲強(qiáng)度 | ASTM D790/ISO 178 | 152 | kg/cm2(MPa)[Lb/in2] | ||
IZOD 缺口沖擊強(qiáng)度 | 1/4" 23℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||
1/4" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
1/8" 23℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
1/8" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
Charpy沖擊強(qiáng)度 | 23℃ (缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||
-30℃(缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
23℃(無缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
-30℃(無缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
物性性能 | 比重(密度) | ASTM D792/ISO 1183 | 1.60 | ||
吸水率 23℃/24H | ASTM D570/ISO 62 | % | |||
熱性能 | 熱變形溫度 | 退火 | ASTM D648/ISO 75 | ℃(℉) | |
未退火 | ASTM D648/ISO 75 | 355 | ℃(℉) | ||
熔點(diǎn) | - | ℃(℉) | |||
燃燒性(率) | UL94 | ||||
線性膨脹系數(shù) | ASTM D696/ISO 11359 | mm/mm.℃ | |||
電氣性能 | 介電常數(shù) | 100HZ | ASTM D150/IEC 60250 | ||
1MHZ | ASTM D150/IEC 60250 | ||||
介電損耗 | 100HZ | ASTM D150/IEC 60250 | |||
1MHZ | ASTM D150/IEC 60250 | ||||
體積電阻率 | ASTM D257/IEC 60093 | Ω.cm | |||
表面電阻率 | ASTM D257/IEC 60093 | Ω | |||
耐電弧性 | ASTM D495/IEC 60112 | ||||
加工條件 | 干燥條件 | ||||
加工溫度 | 射嘴 | ℃ | |||
料筒前段 | ℃ | ||||
料筒中段 | ℃ | ||||
料筒后段 | ℃ | ||||
熔體溫度 | ℃ | ||||
模具溫度 | ℃ | ||||
壓力 | 注塑壓力 | Mpa | |||
保壓壓力 | Mpa | ||||
背壓 | Mpa | ||||
螺桿轉(zhuǎn)速 | rpm | ||||
其他 | 備注 | ||||
顏色 | |||||
特性 | 低粘度 耐化學(xué)性良好 耐熱性高 剛性高 耐磨損性良好 | ||||
用途 | 電氣電子應(yīng)用領(lǐng)域 光學(xué)數(shù)據(jù)存儲(chǔ) 線圈骨架 |