K膠臺灣奇美PB-5903 物性表:
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
物理性能 | 比重 | 23℃ | ASTM D-792 | 1.02 | --- |
濁度 | 1/8 | ASTM D-1003 | 1.5 | --- | |
光線透光率 | 1/8 | ASTM D-1003 | 90.5 | % | |
機(jī)械性能 | 硬度 | --- | Shore D | 67 | --- |
引張強(qiáng)度 | 1/8 | ASTM D-638 | 250 | kg/cm2 | |
彎曲強(qiáng)度 | 1/4 | ASTM D-790 | 320 | kg/cm2 | |
彎曲彈性率 | 1/4 | ASTM D-790 | 14000 | kg/cm2 | |
IZOD沖擊強(qiáng)度 | 1/4",23℃ | ASTM D-256 | 3.0 | kg.cm/cm | |
加工性能 | 流動系數(shù) | 200℃,5Kg | ASTM D-1238 | 10 | g/10min |
熱 性 能 | 維卡軟化點 | 1/8 | ASTM D-1525 | 87 | ℃ |
熱變形溫度 | 1/4",120℃/hr | ASTM D-648 | 71 | ℃ |