產(chǎn)品參數(shù)
?
?
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 吸水率 | 24hr,in 23℃ | ASTM D-570 | 0.20 | % | |
物理性能 | 折射率 | ASTM D-542 | 1585 | |||
透光率 | 3mm thick | ASTM D-1003 | 88 | |||
阻燃性 | 0.38mm | UL 94 | V-2 | |||
比重 | JIS K-7112 | 1.20 | ||||
機械性能 | 拉伸模量 | ASTM D-638 | 2120(21600) | Mpa(kgf/cm2) | ||
彎曲模量 | ASTM D-790 | 2230(22700) | Mpa(kgf/cm2) | |||
拉伸率 | 屈服點 | ASTM D-638 | 6 | % | ||
斷裂點 | ASTM D-638 | 140 | % | |||
彎曲強度 | ASTM D-790 | 90(915) | Mpa(kgf/cm2) | |||
耐沖擊強度值 | 艾氏、帶缺口厚度3.2mm | ASTM D-256 | 880(90) | J/m(kgf·cm/cm) | ||
壓縮強度 | ASTM D-695 | 76(770) | Mpa(kgf/cm2) | |||
洛氏硬度 | ASTM D-785 | 77 | M標度 | |||
耐沖擊強度值 | 艾氏、帶缺口厚度6.4mm | ASTM D-256 | 140(14) | J/m(kgf·cm/cm) | ||
拉伸強度 | 屈服點 | ASTM D-638 | 61(620) | Mpa(kgf/cm2) | ||
斷裂點 | ASTM D-638 | 81(830) | Mpa(kgf/cm2) | |||
電氣性能 | 介電率 | 60Hz | ASTM D-150 | 2.95 | ||
耐電弧性 | ASTM D-495 | 110 | sec | |||
介電正切 | 106Hz | ASTM D-150 | 0.009 | |||
絕緣破壞強度 | 快速加壓值厚度1.6mm | ASTM D-149 | 30 | kv/mm | ||
介電正切 | 60Hz | ASTM D-150 | 0.0004 | |||
介電率 | 106Hz | ASTM D-150 | 2.9 | |||
耐導(dǎo)電徑跡性(CTI) | IEC 112 | 300 | V | |||
體積電阻率 | ASTM D-257 | 3×1016 | Ω.cm | |||
加工性能 | 成型收縮率 | 流動方向 | ASTM D-955 | 0.5~0.7 | % | |
垂直方向 | ASTM D-955 | 0.5~0.7 | % | |||
熱性能 | 溫度指數(shù) | 電學(xué)式 | 厚度1.47mm | UL 746B | 125 | ℃ |
沖擊式 | 厚度1.47mm | UL 746B | 115 | ℃ | ||
非沖擊式 | 厚度1.47mm | UL 746B | 125 | ℃ | ||
線膨脹系數(shù) | 流動方向 | ASTM D-696 | 7 | 10-5cm/cm/℃ | ||
垂直方向 | ASTM D-696 | 7 | 10-5cm/cm/℃ | |||
負荷撓曲溫度 | 負荷1.813MPa(18.6kgf/cm2) | JIS K-7207 | 133 | ℃ | ||
負荷撓曲溫度 | 負荷0.451MPa(4.6kgf/cm2) | JIS K-7207 | 143 | ℃ |