PPS A674M2 日本東麗工業(yè)株式會社 物性數(shù)據(jù) |
①原料描述部分 |
|||
規(guī)格級別: |
--- |
外觀顏色: |
--- |
用途概述: |
--- |
||
備注說明: |
特性:高抗沖擊,與彈性體合金類型:特殊 |
②原料技術(shù)數(shù)據(jù) |
|||||||||||||
性能項目 |
試驗條件[狀態(tài)] |
測試方法 |
測試數(shù)據(jù) |
數(shù)據(jù)單位 |
|||||||||
基本性能 |
吸水率 |
--- |
ASTM D-570 |
0.02 |
% |
||||||||
物理性能 |
比重 |
--- |
ASTM D-792 |
1.56 |
--- |
||||||||
|
--- |
|
|
|
|||||||||
流動長 |
320℃,98MPa,1mm厚 |
東麗法 |
80 |
×10-3m |
|||||||||
機械性能 |
引張強度 |
--- |
ASTM D-638 |
150 |
MPa |
||||||||
拉伸強度 |
--- |
ASTM D-638 |
2.9 |
% |
|||||||||
彎曲強度 |
--- |
ASTM D-790 |
220 |
MPa |
|||||||||
彎曲彈性體 |
--- |
ASTM D-790 |
10.0 |
GPa |
|||||||||
斷裂強度 |
--- |
ASTM D-732 |
65 |
--- |
|||||||||
|
--- |
|
|
|
|||||||||
硬度 |
--- |
ASTM D-785 |
114 |
洛氏 |
|||||||||
摩耗 |
--- |
ASTM D-1044 |
50 |
mg/1000回 |
|||||||||
摩擦系數(shù) |
對鋼 |
ASTM D-1894 |
0.25 |
--- |
|||||||||
限界PV值 |
--- |
東麗法 |
815 |
kj/m2.hr |
|||||||||
電氣性能 |
耐電弧性W電級 |
--- |
ASTM D-495 |
120 |
秒 |
||||||||
體積固有抵抗 |
--- |
ASTM D-257 |
1016 |
Ω.m |
|||||||||
絕緣破壞電壓 |
--- |
ASTM D-149 |
17 |
MV/m |
|||||||||
誘電率 |
106Hz |
ASTM D-150 |
6.0 |
--- |
|||||||||
誘電正接 |
106Hz |
ASTM D-150 |
0.004 |
--- |
|||||||||
熱 性 能 |
融點 |
--- |
DSC |
278 |
℃ |
||||||||
熱變形溫度 |
1.82MPa |
ASTM D-648 |
>260 |
℃ |
|||||||||
|
--- |
|
|
|
|||||||||
燃燒性 |
--- |
UL-94 |
V-0(1/8") |
--- |