主要用于電鍍表面、強(qiáng)化表面、真空電鍍表面.PU表面.UV表面等材料上,具有高色澤、高色彩、高遮蓋力、高穩(wěn)定性、耐酒精及耐磨擦之特點(diǎn)。 印刷:絲印移印均可。 表干及實干時間:表干時間自然揮發(fā)5-10分鐘;實干時間在24小時以內(nèi)。 稀釋及清洗:SV3慢干開油水、UVK1(移印開油水)同時可使用718洗網(wǎng)水清洗。 測試方法(完全干燥后): 1、3m膠紙粘在畫有百格的表面,45度角迅速拉起不脫油; 2、純度99%的工業(yè)酒精,一千克砝碼用棉布包住在表面,以水平力來回拉200次無脫色; 3、 耐磨:橡皮擦500g力水平來回擦500次。 使用方法: 1、使用前應(yīng)充分?jǐn)嚢?,用后隨時封閉; 2、攪拌時加開油水10-15%,稀釋到印刷粘度; 3、網(wǎng)板塞網(wǎng)時可用洗網(wǎng)水清洗; 4、不得與其它類型混合使用。 注意事項: 1、塑膠材料的外觀相似,但可能會是不同的材料,客戶需試印確定其符合要求后,再批量印刷; 2、在移印過程中,如出現(xiàn)拉絲或散開,可適當(dāng)加入一些慢干膏即可; 3、環(huán)境溫度過高,將會影響原有質(zhì)量; 4、根據(jù)氣候變化,請遠(yuǎn)離火源,陰暗環(huán)境下存放。
Oles MPE Plating Ink
MPE plating strengthening series ink characteristics : mainly used in plating surface, enhanced surface, vacuum plating surface.PU surface.UV surface and other materials, with a high color, high color, high covering power, high stability, high alcohol and rub characteristics. Printing: screen printing can be. Surface drying and drying time: surface dry time natural volatile 5-10 minutes; work time within 24 hours. Dilution and cleaning: SV3 slow dry open water, UVK1 ( printing open water) can be simultaneously used 718 washing network water cleaning. Test method ( completely dry ): 1, 3M gummed paper in the paintings of the surface of the ink, 45 degree angle quickly pulled off the oil; 2, 99% of the purity of industrial alcohol, one kilogram of weight of cotton pack in the ink surface, with a horizontal force pulling back and forth 200 times without decolorization; 3: oak, wear resistance eraser 500g force level brush back and forth 500 times. Usage: 1, use should be fully stirred, use at any time after the closure; 2, add water mixing 10-15%, diluted to 3, screen printing viscosity; the plug is available when washing network water cleaning; 4, not with other types of ink mixing. Note: 1, the plastic material similar in appearance, but may be of different materials, customers need to try to determine its requirements, and then batch printing; 2, in the printing process, such as drawing or spread out, may be appropriate to add some slow dry plaster; 3, the ambient temperature is too high, will affect the quality of the original ink; 4, according to climate change, please stay away from fire, dark environment storage.